CATEGORY
OUR PRODUCTS
KL-3G(Brightener)
PRODUCT DESCRIPTION
Composition: high-efficiency surfactant, fatty acid derivatives, etc.
Appearance: granular or powdery, white to light yellow, light red
Packing: double-layer packaging in plastic bag, composite woven paper bag
Net weight: 25kg/bag
Storage time limit: stored in a ventilated, dry, non-corrosive warehouse for two years
Safety performance: odorless, non-toxic, non-polluting
PH value: 5.5-9.5
Heating loss (55℃): ≤2.0%
Inorganic content (950℃): ≤16.0%
APPLICABLE SCOPE
Suitable for natural rubber, synthetic rubber and reclaimed rubber.
PERFORMANCE CHARACTERISTICS
1. When KL-3G is mixed with rubber compound according to the recommended ratio, it can improve the appearance characteristics of rubber products, and the surface brightness of the products can be greatly improved.
2. When KL-3G is used, it has a good release effect, which can keep the mold clean and bright, prolong the cleaning cycle of the mold, and have an excellent improvement effect on the contamination, stain and corrosion of the mold.
3. KL-3G can improve the fluidity of the rubber compound, increase the calendering or extrusion speed during mixing, and has the function of processing dispersant, which can not only make the index of each batch of products uniform, maintain high stability of product quality, but also Significantly reduce production energy consumption, but also improve product yield to achieve the goal of reducing overall costs.
4. KL-3G has good compatibility with the rubber compound, and its use within the recommended dosage will not affect the hardness, tensile strength, definite elongation strength and other physical properties of the rubber product.
5. KL-3G Adding KL-3G in the rubber injection and molding process can make the surface of the extruded rubber material smooth and flat, with a delicate appearance and accurate size, and improve the internal and external quality of the product.
INSTRUCTIONS FOR USE
1. It can be added together with other chemical compounding agents during the mixing process, which can play the role of dispersing flow and demoulding.
2. It is added in the late stage of mixing, and the effect of demoulding and brightening is better.
DOSAGE RECOMMENDED
1. General raw rubber: add 1 to 4 parts according to the amount of raw rubber.
2. Halogenated rubber and other polar adhesives: the dosage should be appropriately increased.
If you are interested in our products, welcome to leave us a message.
Related Products
CARBON BLACK DISPERSANT FOR TYRES TIRES
Email: market@allwardtech.com
Mob/WP/WeChat: 0086 150 6301 2586
Address: Rm 1402 No.860 Hefei Road, Laoshan District, Qingdao, China