CATEGORY
OUR PRODUCTS
KT-8B
PRODUCT DESCRIPTION
Composition: Mixture of metal soap salt and organic functional polymer resin
Appearance: powdery or granular, light tan, tan or dark tan
Packing: double-layer packaging in plastic bag, composite woven paper bag
Net weight: 25kg/bag
Storage time limit: stored in a ventilated, dry, non-corrosive warehouse for two years
Safety performance: non-toxic, harmless
APPLICABLE SCOPE
Suitable for natural rubber, synthetic rubber and reclaimed rubber. Both sulfur vulcanization and peroxide vulcanization are applicable.
Application areas: 1. All-steel and semi-steel tires 2. Motorcycle tires 3. Conveyor belts, hoses, shoes 4. Various seals
PERFORMANCE CHARACTERISTICS
1. KT-8B can effectively improve the mixing effect of the rubber compound, effectively speed up the dispersion of carbon black and other fillers in the rubber compound, further shorten the mixing time, improve the extrusion and calendering speed, and reduce energy consumption to achieve The goal of reducing production costs.
2. KT-8B can effectively reduce the Mooney viscosity of the compounded rubber, improve the fluidity of the rubber compound, improve the compactness and brightness of the extruded and calendered products, reduce the defects of the finished products, and improve the appearance quality and qualification of the products. Rate.
3. The use of KT-8B helps to improve scorch performance and improve the safety of rubber compound processing operations. At the same time, adding an appropriate amount is also beneficial for improving the wear resistance and flexural cracking performance of the finished product.
4. KT-8B can greatly improve the stability of product batch indicators, and can obtain products with stable dimensions and delicate appearance, and can also improve the yield of products to achieve the goal of reducing overall costs.
5. KT-8B has good compatibility with various rubbers. Under the premise of the recommended dosage, it has no adverse effect on the physical properties of the product. It can be widely used in the ingredients of various rubbers. The frosting of the material is beneficial.
INSTRUCTIONS FOR USE
KT-8B can be added together with other chemical compounding agents during the mixing process, and the effect of adding it in advance is better.
DOSAGE RECOMMENDED
1. Add 1~4 parts of the raw rubber amount.
2. The amount of polar glue is appropriately increased.
If you are interested in our products, welcome to leave us a message.